- Description
- Application
A heterogeneous cation-exchange membrane. The polymer backbone of this membrane is based on A Proprietary hydrocarbon resin. The mechanical reinforcement is composed of polypropylene (also known as PP) and it has the open mesh style.
Electrocoating, electroplating, electrodeionisation, electrodialysis for demineralisation, desalination and others.
Backing Foil | None |
---|---|
Bubble Point | >3 bar (in H2O at 25°C) |
Characteristics | High selectivity and very high mechanical stability. |
Conductivity | >1.7 mS/cm |
Counter Ion | Sodium (Na+) |
Delivery Condition | Dry (Delivery form) |
Exchange Capacity | 1.6 meq/g |
Membrane Appearance | Brown |
Permselectivity | >93% |
pH | 1-10 pH (Stability Range at 25°C) |
Reinforcement | PP (polypropylene fabrics) |
Resistance | < 30.0 Ω·cm2 (Specific area resistance) |
Size | 10cm x 10cm, 20cm x 30cm |
Swelling | < 2% (in H2O at 25°C) (Dimensional Swelling) |
Thickness | 450-500 µm |
Transfer Rate | >50 nmol·min-1·cm-2 (Hydroxyl Transfer Rate) |